Emkhakheni we-die-casting, wonke umuntu uyazi ukuthi ukukhubazeka ebusweni bezingxenye zokufa kujwayelekile, futhi kunezinhlobo eziningi zokukhubazeka, futhi amagama ahlukile ezindaweni ezahlukahlukene, njengama-flow marks, kanti amanye abizwa ngama-streaks. Okudidayo ukuthi akhiqizwa kanjani ama-flow marks of die castings, ngabe ikhona indlela yokuwaxazulula? Yimaphi amamaki wokugeleza ekufeni?
Isici esiyinhloko sophawu lokugeleza kokusakazwa kokufa ukuthi ubuso bokuphonsa buveza iphethini elibushelelezi lokudangala ngokwengxenye okuhambisana nokuhamba kokugeleza kwensimbi encibilikile futhi kungazwakala ngesandla. Ukukhubazeka kwamamaki okugeleza akunasiqondisi sentuthuko futhi kungasuswa ngezindlela zokupholisha.
Ngabe kwenzeka kanjani amamaki okugeleza kokufa?
Ukuhlaziywa kwezizathu eziningana zamamaki wokugeleza:
Iminonjana eshiywe yimifudlana emibili yensimbi egcwalisa umgodi ngaphandle kokuvumelanisa;
Izinga lokushisa eliphansi lesikhunta, njenge-zinc ingxubevange yokushisa kwesikhunta <150 ° C kanye ne-aluminium ingxubevange lokushisa <180 ° C, kuthambekele kokukhubazeka okunjalo;
Ijubane lokugcwalisa liphezulu kakhulu;
Upende owedlulele.
Ungakuqeda kanjani ukukhubazeka kokumaka kokugeleza ekufeni?
Isixazululo:
Lungisa indawo enqamulelayo noma ukuma kwesango;
Lungisa izinga lokushisa lesikhunta futhi wandise inkatho yokuchichima;
Lungisa kahle ijubane lokugcwalisa ukushintsha isimo soketshezi lwensimbi yokugcwalisa insimbi encibilikisiwe;
Ukumboza kuncane futhi kufana.
Sicela ugcine umthombo nekheli lale ndatshana ukuze uphinde uprintwe: Izimbangela Zamamaki Okugeleza E-Die Castings Nezindlela Zabo Zokuqeda
UMinghe Inkampani yeDie Casting anikezelwe ekukhiqizeni nasekuhlinzekeni ikhwalithi nokusebenza okuphezulu Izingxenye Zokulingisa (izingxenye zensimbi zensimbi zokufa zisebenza ikakhulukazi zibandakanya I-Thin-Wall Die Casting,I-Hot Chamber Die Casting,Cold Chamber die Casting), Insizakalo Eyindilinga (Insiza Yokulingisa,ICnc Machining,Ukwenza Okubandayo, Surface Treatment) .Noma ikuphi ukusakazwa kwe-Aluminium die, i-magnesium noma i-Zamak / zinc die casting nezinye izidingo zokuphosa zamukelekile ukuxhumana nathi.
Ngaphansi kokulawulwa kwe-ISO9001 ne-TS 16949, Zonke izinqubo zenziwa ngamakhulu emishini esezingeni eliphakeme yokufa, imishini ye-5-axis, nezinye izikhungo, ezisukela kuma-blasters kuya kumishini yokuwasha ye-Ultra Sonic.Minghe akagcinanga ngemishini esezingeni eliphezulu kepha futhi unobuchwepheshe iqembu lonjiniyela abanolwazi, ama-opharetha nabahloli ukwenza ukwakheka kwekhasimende kugcwaliseke.
Umenzi wenkontileka yokufa kwabasikiwe. Amandla afaka izingxenye ezibandayo ze-aluminium die casting ezivela ku-0.15 lbs. kuye ku-6 lbs., Ukusetha ushintsho olusheshayo, nemishini. Izinsizakalo ezingezwe ngenani zifaka phakathi ukupholisha, ukudlidliza, ukuphazamisa, ukuqhumisa ngokudubula, ukupenda, ukuhlobisa, ukumboza, ukuhlangana nokusetshenziswa kwamathuluzi. Izinto zokusebenza ezisetshenzisiwe zifaka ama-alloys afana no-360, 380, 383, no-413.
I-Zinc die casting design usizo / izinsizakalo zobunjiniyela ezihambisanayo. Umenzi wangokwezifiso we-precision zinc die castings. Ukusakazwa okuncane, ukukhishwa kwengcindezi ephezulu, ukusikeka kwesikhunta esiningi, ukujikijelwa kwesikhunta okuvamile, ukufefa kwamayunithi kanye nokuzimela okuzimele kanye nokuvalwa okuvaliwe komgodi kungenziwa. Ama-Castings angenziwa ngobude nobubanzi obufinyelela ku-24 in. Ku +/- 0.0005 in. Ukubekezelelana.
I-ISO 9001: Umkhiqizi oqinisekisiwe ka-2015 we-die cast magnesium, Amandla afaka i-high-pressure magnesium die casting up to 200 ton chamber hot & 3000 ton cold chamber, designing designing, polishing, molding, machining, powder & liquid paint, QA full with CMM amakhono , inhlangano, ukupakisha nokulethwa.
Kuqinisekiswe i-ITAF16949. Insiza Eyengeziwe Yokulingisa Faka ukukhipha utshalomali,ukuphonsa kwesihlabathi,Ukuphonswa kwamandla, Lost Foam Ekubunjweni,I-Centrifugal Casting,Ukuphoswa Kokuqothula,Permanent Isikhunta Ukulingisa, Amakhono afaka i-EDI, usizo lobunjiniyela, ukumodeliswa okuqinile nokucutshungulwa kwesibili.
Izimboni Zokulingisa Izingxenye Zamacala Ezifundo Zezimoto: Izimoto, Amabhayisikili, Izindiza, Izinsimbi Zomculo, I-Watercraft, Amadivayisi we-Optical, Izinzwa, Amamodeli, Amadivayisi we-elekthronikhi, Ukuvaleka, Amawashi, Imishini, Izinjini, Ifenisha, Ubucwebe, AmaJig, Telecom, Ukukhanyisa, Amadivayisi Wezokwelapha, amadivayisi wezithombe, Amarobhothi, okubaziwe, okokusebenza komsindo, okwezemidlalo, i-Tooling, Amathoyizi nokuningi.
Yini esingakusiza ukuthi uyenze ngokulandelayo?
∇ Iya ekhasini eliyisiqalo For I-Die Casting China
→Izingxenye Zokusakaza-Thola esikwenzile.
→ Izeluleko Ezilinganisiwe Mayelana Izinsizakalo Zokufa Zokusakaza
By Umkhiqizi weMinghe Die Casting | Izigaba: Izindatshana Eziwusizo |Material Omaka: I-Aluminium Casting, Zinc Ukulingisa, Ukulingiswa kweMagnesium, I-Titanium Casting, Insimbi Engagqwali, Brass Ekubunjweni,Ukulingiswa kweBronze,Isakaza ividiyo,Umlando wenkampani,I-Aluminium Die Casting | Amazwana Off