Isixazululo Sokumanzi Okumanzi Esikhathini Esiphakathi Sokungeniswa Kwemvamisa Ephakathi
I-Furnace knotting inqubo ebalulekile ekusetshenzisweni kokuncibilikisa nasekuphonseni iziko eliphakathi nendawo lokungeniswa. Eminyakeni edlule, ukuphindwaphindwa kokwenziwa kwesithando somlilo nokuthengwa kwesithando somlilo bekunganelisi. Sisebenzisa ubuchwepheshe obumanzi obufuthayo besithando somlilo samandla aphakathi nendawo, esithuthukiswe kahle.
I-1. Izinzuzo
Ubuchwepheshe bokubopha obumanzi besithando sokungeniswa semvamisa esiphakathi nobuchwepheshe obusha bokubopha ifindo lesithando somlilo esivele eminyakeni yamuva. Ngemuva kokwethulwa enkampanini yethu ngonyaka we-2012, ngemibhikisho ebucayi eyandulelayo, siphumelele ekushoneni okukodwa, futhi saxazulula inkinga yokusebenza ngamandla okukhulu, okudla isikhathi, kanye nekhwalithi eyindida ebhekene nomsebenzi wethu wokubopha isithando somlilo. Ngaphezu kwalokho, le ndlela yokubopha isithando somthambo futhi kulula ukuyiqaqa, futhi impilo yensizakalo icishe ifane naleyo eyomile. Isithando somlilo esingu-1t singaqinisekisa ukuncibilika okuphephile kwensimbi ebunjiweyo engaphezu kwama-60t njalo.
2. Indlela eyisisekelo
Esigabeni sokuqala sokufaka isicelo, sisebenzise isihlabathi se-silica njengezinto eziyisisekelo zento yokwakheka kwesithando somlilo. Izithako eziyisisekelo yilezi: isihlabathi se-silica: 2 # (8 - 10 mesh) 5%, 3 # (10 - 26 mesh) 35%, 4 # (16 ~ 24 mesh) 35%, 8 # (250 ~ 400 mesh) 25 %; I-Boric acid: 2.5%; amanzi: 8%. Ngemuva kokwakhiwa kabusha okomile okuthathu nokomanzi okumanzi, ifindo likhiywa kancane kancane emlonyeni wesithando ngokusebenzisa induku yokudlidliza ngenkathi udla. Ngemuva kokumiswa kwemvelo kwe-4-6h (kuya ngethempelesha), khipha isikhunta sensimbi, bese usomisa ngokwemvelo kungabi ngaphansi kuka-2h (kuya ngethempelesha, uma kungenzeka, isikhathi sokomisa semvelo singanwetshwa sifike ku-8-10h okuhle kakhulu). Ngemuva kokuqeda ukhololo wesithando somlilo, faka amapayipi wensimbi ayi-6-8 esithandweni somlilo odongeni lomlilo, bese ufaka ipayipi lensimbi (elinesisekelo) phakathi, bese uqala i-ovini yamandla. Imininingwane yehhavini iyafana naleso sesithando somlilo esomile.
3. Qhathanisa
Uma kuqhathaniswa nesithando somlilo esomile, isithando somswakama esinamanzi asinazo izingqimba zesendlalelo ezingaba khona esithandweni esomile. Inkokhelo yesithando somlilo yengezwa isikhathi ngasinye igcwaliswa ngokulinganayo ngaphansi kwenduku yokudlidliza, futhi amanzi amaningi aqhubeka nokukhuphuka, aqinisekisa ukuthi ukuhlanganiswa kwemali esanda kufakwa esithandweni kanye nemali yokuqala yesithando somlilo ayihlukani. Ikakhulukazi ngemuva kwalokho, sisebenzise i-mixer ukuhlanganisa izinto zesithando somlilo, sayiqeda nya inkinga yokuqina kwesithando somlilo. Ukuphawula isithando somlilo akulula nje kuphela, kodwa futhi nekhwalithi ingaqinisekiswa ngokuphelele. Manje sisebenzisa i-refractory aggregate (uhlobo oluthile lokulungiswa kwesithando somlilo) esikhiqizwa yifektri yobungcweti ukwenza kube lula ukubopha isinye somlilo. Okuwukuphela kwephutha ukuthi amandla omzimba awaphakeme njengalawo esithandweni esomile, kepha inqobo nje uma umsebenzi wokuncibilikisa wenziwa ngokwezimpawu zawo, ukushiyeka kwawo akuyona inkinga.
4. Amaphuzu ezobuchwepheshe
Amaphuzu ezobuchwepheshe okufanele uwaqaphele lapho usebenzisa isithando somlilo esimanzi:
- (1) Ukubanjwa komswakama wentengo eshukumisayo kufanele kube kome kunokuba kube manzi, ukuze kugwenywe ukuchichima komswakama okweqile ngesikhathi sokuklina.
- (2) Ihhavini kufanele lenziwe ngokwehlukana, kanti i-ovini elenziwe ngezinto alinakwenziwa. Ngokuncibilikisa kokuqala, ikakhulukazi ukushaja kokuqala kwenkokhiso, inkokhiso kufanele ishaye phansi nodonga lwesithando ngangokunokwenzeka. Ngezinye izikhathi, gwema ukusebenzisa udonga lwesithando njengesisekeli sokuhambisa imali.
- (3) Uma ungeza ukukhokhiswa kwesithando somlilo, naka ngokukhethekile ukugwema okokusebenza okuchithiwe ukugwema ukuvela kokusebenza kokushintsha kwezinto.
- (4) Lapho isithando somlilo siwa kancane, sihlikihle ngengilazi yamanzi bese usixhuma uvalwe ngento emanzi yesithando somlilo.
Ukuphetha amazwi
Umkhuba weminyaka eminingana ukhombisile ukuthi ubuchwepheshe obumanzi bokusika isithando somlilo kuyindlela elula, ethembekile nephephile yokwakheka kwesithando somlilo, engasetshenziswa ngamabhizinisi ngokuzethemba.
Sicela ugcine umthombo nekheli lale ndatshana ukuze uphinde uprintwe: Isixazululo Sokumanzi Okumanzi Esikhathini Esiphakathi Sokungeniswa Kwemvamisa Ephakathi
UMinghe Inkampani yeDie Casting anikezelwe ekukhiqizeni nasekuhlinzekeni ikhwalithi nokusebenza okuphezulu Izingxenye Zokulingisa (izingxenye zensimbi zensimbi zokufa zisebenza ikakhulukazi zibandakanya I-Thin-Wall Die Casting,I-Hot Chamber Die Casting,Cold Chamber die Casting), Insizakalo Eyindilinga (Insiza Yokulingisa,ICnc Machining,Ukwenza Okubandayo, Surface Treatment) .Noma ikuphi ukusakazwa kwe-Aluminium die, i-magnesium noma i-Zamak / zinc die casting nezinye izidingo zokuphosa zamukelekile ukuxhumana nathi.
Ngaphansi kokulawulwa kwe-ISO9001 ne-TS 16949, Zonke izinqubo zenziwa ngamakhulu emishini esezingeni eliphakeme yokufa, imishini ye-5-axis, nezinye izikhungo, ezisukela kuma-blasters kuya kumishini yokuwasha ye-Ultra Sonic.Minghe akagcinanga ngemishini esezingeni eliphezulu kepha futhi unobuchwepheshe iqembu lonjiniyela abanolwazi, ama-opharetha nabahloli ukwenza ukwakheka kwekhasimende kugcwaliseke.
Umenzi wenkontileka yokufa kwabasikiwe. Amandla afaka izingxenye ezibandayo ze-aluminium die casting ezivela ku-0.15 lbs. kuye ku-6 lbs., Ukusetha ushintsho olusheshayo, nemishini. Izinsizakalo ezingezwe ngenani zifaka phakathi ukupholisha, ukudlidliza, ukuphazamisa, ukuqhumisa ngokudubula, ukupenda, ukuhlobisa, ukumboza, ukuhlangana nokusetshenziswa kwamathuluzi. Izinto zokusebenza ezisetshenzisiwe zifaka ama-alloys afana no-360, 380, 383, no-413.
I-Zinc die casting design usizo / izinsizakalo zobunjiniyela ezihambisanayo. Umenzi wangokwezifiso we-precision zinc die castings. Ukusakazwa okuncane, ukukhishwa kwengcindezi ephezulu, ukusikeka kwesikhunta esiningi, ukujikijelwa kwesikhunta okuvamile, ukufefa kwamayunithi kanye nokuzimela okuzimele kanye nokuvalwa okuvaliwe komgodi kungenziwa. Ama-Castings angenziwa ngobude nobubanzi obufinyelela ku-24 in. Ku +/- 0.0005 in. Ukubekezelelana.
I-ISO 9001: Umkhiqizi oqinisekisiwe ka-2015 we-die cast magnesium, Amandla afaka i-high-pressure magnesium die casting up to 200 ton chamber hot & 3000 ton cold chamber, designing designing, polishing, molding, machining, powder & liquid paint, QA full with CMM amakhono , inhlangano, ukupakisha nokulethwa.
Kuqinisekiswe i-ITAF16949. Insiza Eyengeziwe Yokulingisa Faka ukukhipha utshalomali,ukuphonsa kwesihlabathi,Ukuphonswa kwamandla, Lost Foam Ekubunjweni,I-Centrifugal Casting,Ukuphoswa Kokuqothula,Permanent Isikhunta Ukulingisa, Amakhono afaka i-EDI, usizo lobunjiniyela, ukumodeliswa okuqinile nokucutshungulwa kwesibili.
Izimboni Zokulingisa Izingxenye Zamacala Ezifundo Zezimoto: Izimoto, Amabhayisikili, Izindiza, Izinsimbi Zomculo, I-Watercraft, Amadivayisi we-Optical, Izinzwa, Amamodeli, Amadivayisi we-elekthronikhi, Ukuvaleka, Amawashi, Imishini, Izinjini, Ifenisha, Ubucwebe, AmaJig, Telecom, Ukukhanyisa, Amadivayisi Wezokwelapha, amadivayisi wezithombe, Amarobhothi, okubaziwe, okokusebenza komsindo, okwezemidlalo, i-Tooling, Amathoyizi nokuningi.
Yini esingakusiza ukuthi uyenze ngokulandelayo?
∇ Iya ekhasini eliyisiqalo For I-Die Casting China
→Izingxenye Zokusakaza-Thola esikwenzile.
→ Izeluleko Ezilinganisiwe Mayelana Izinsizakalo Zokufa Zokusakaza
By Umkhiqizi weMinghe Die Casting | Izigaba: Izindatshana Eziwusizo |Material Omaka: I-Aluminium Casting, Zinc Ukulingisa, Ukulingiswa kweMagnesium, I-Titanium Casting, Insimbi Engagqwali, Brass Ekubunjweni,Ukulingiswa kweBronze,Isakaza ividiyo,Umlando wenkampani,I-Aluminium Die Casting | Amazwana Off