I-Operation Nezinyathelo Zokuqothula I-Flame Heating Surface Quenching
Insimbi yensimbi, insimbi yensimbi, ingxubevange yensimbi ingafudunyezwa kancane ifike cishe ku-300 ~ 500ºC ngombhobho ocimayo onamalangabi amancane ukuvimbela ukuqhekeka. Ukushisa okucimayo kwezingxenye zensimbi yi-Ac3 + (80 ~ 100ºC), kanye nokushisa okucishayo kokuphonsa insimbi ingu-730ºC + 28 × ωSi ºC -25 × ωMnºC. ...