Izinzuzo Nobubi Of Free UKWAKHA Futhi Die UKWAKHA Izindlela
UKWAKHA Mahhala
UKWAKHALA kwamahhala kubhekisa kunqubo yokucubungula yama-forgings asebenzisa amathuluzi alula enhloso ejwayelekile noma asebenzise ngqo amandla wangaphandle kokungenalutho phakathi kwama-anvils aphezulu naphansi wemishini yokwakha ukuze kukhubazwe okungenalutho ukuthola umumo wejometri odingekayo nekhwalithi yangaphakathi. Ama-forgings akhiqizwa yindlela yokukhwabanisa yamahhala abizwa ngama-forgings wamahhala.
UKWAKHA kwamahhala ikakhulu kukhiqiza amaqoqo amancane we-forgings. Imishini yokwakha efana nezando zokwakha nemishini ye-hydraulic isetshenziselwa ukwakha izikhala ukuthola ama-forgings afanelekile. Izinqubo eziyisisekelo zokufaka mahhala zifaka ukucasula, ukudweba, ukushaya isibhakela, ukusika, ukugoba, ukusonta, ukuguqula nokufaka okuthile. UKWAKHA Mahhala usebenzisa indlela ekwakheni eshisayo.
Inqubo yokwakha yamahhala ifaka izinqubo eziyisisekelo, izinqubo ezisizayo, nezinqubo zokuqeda.
- Izinqubo eziyisisekelo zokwakha mahhala: ukucasula, ukudweba, ukushaya isibhakela, ukugoba, ukusika, ukusonta, ukuguqula nokufaka okuthile, njll. Okusetshenziswa kakhulu ekukhiqizeni kwangempela izinqubo ezintathu zokucasula, ukudweba nokushaya.
- Inqubo Yokusiza: inqubo yangaphambi kokumosheka, njengokucindezela imihlathi, ukucindezela imiphetho yensimbi yensimbi, ukusika amahlombe, njll.
- Inqubo yokuqedela: inqubo yokunciphisa ukukhubazeka ebusweni bokufaka, njengokukhipha indawo engalingani yokwakha nokubumba.
Izinzuzo zokwakhiwa kwamahhala: ukukhiqizwa okukhulu kokuguquguquka okukhulu, izingxenye ezincane ezingaphansi kuka-100kg zingakhiqizwa, futhi izingxenye ezisindayo ezifika ku-300t noma ngaphezulu zingakhiqizwa; amathuluzi asetshenzisiwe amathuluzi alula ajwayelekile; ekwakheni ukwakha iwukuba kancane okhubaza blank ezindaweni ezihlukene, ngakho-ke, UKWAKHA Ngokufanayo, the tonnage imishini ekwakheni edingekayo for forgings incane kakhulu kunaleyo imodeli UKWAKHA; izidingo zokunemba kwemishini ziphansi; futhi umjikelezo wokukhiqiza mfushane.
Okubi kanye nemikhawulo yokwakhiwa kwamahhala: ukusebenza kahle kokukhiqiza kuncane kakhulu kunokwakhiwa kwemodeli; i-forgings inezimo ezilula, ukunemba okuphansi kwe-dimensional, nezindawo ezinzima; abasebenzi banamandla aphezulu emisebenzi futhi badinga amazinga aphezulu obuchwepheshe; akulula ukufeza ukusetshenziswa kwemishini nokuzenzekelayo.
Die ekwakheni
I-Die Forging isho indlela yokwakha esebenzisa isikhunta ukwakha okungenalutho kuzinto zokuzinikela zokufa ezizinikele ukuthola ukwakhiwa. Ukuxolelwa okukhiqizwe ngale ndlela kunokulinganisa okuqondile, izibonelelo ezincane zemishini, nezakhiwo eziyinkimbinkimbi nokukhiqiza.
Ngokusho imishini ehlukene esetshenzisiwe: isando die ekwakheni, crank cindezela die ekwakheni, flat ekwakheni umshini die ekwakheni futhi ukuhilizisana cindezela die ekwakheni, njll
Imishini esetshenziswa kakhulu yokwakha isando ifaka isando somoya owakha isando, isando esingeyona i-anvil nesando esinejubane elikhulu.Ingahlukaniswa ngezigaba ezimbili: kufa ukwakha umgodi wokufa nokwenza okungenalutho ukwenza umgodi wokuya ngokuya ngemisebenzi yawo ehlukene.
1) UKWAKHA die wazalela.
- Pre-UKWAKHA die die. Umsebenzi we pre-UKWAKHA die ingaphakathi iwukuba deform blank ukuba seduze ukuma nosayizi UKWAKHA, ukuze ngesikhathi ekwakheni lokugcina, insimbi kalula ukugcwalisa umgodi die ukuthola ubukhulu edingekayo UKWAKHA. Okokuxolelwa okunomumo olula noma lapho i-batch ingekho enkulu, umgodi wokufa wangaphambi kokukhipha ungahlinzekwa. I-fillet kanye nomthambeka womgodi wokufa wangaphambi kokumba mkhulu kakhulu kunalowo womgogodla wokugcina wokukhwabanisa, futhi ayikho i-flash groove.
- Okwakhela okokugcina ukufa kwakufa. Umsebenzi wokugcina ekwakheni die umgodi iwukuba ekugcineni sengozini elingenalutho ukuma edingekayo nosayizi UKWAKHA. Ngakho-ke, ukwakheka kwayo kufanele kufane nokwakha; kepha ngoba ukufakwa kuzoncipha lapho sekupholile, ubukhulu bokugcina bokugcina bokufa kufanele bube bukhulu kunalokho bokufola. Usayizi ukhuliswa ngenani lokuncipha. Ukuncipha kwensimbi ye-forgings kuthathwa njenge-1.5%. Ngaphezu kwalokho, kukhona ama-flash grooves eceleni komngcele wesikhunta ukwandisa ukumelana nensimbi ephuma emgodini wesikhunta, ukukhuthaza insimbi ukugcwalisa umgodi wesikhunta, futhi ngesikhathi esifanayo ukufaka insimbi eningi.
2) elingenalutho okwenza isikhunta umgodi.
Kwama-forgings anezimo eziyinkimbinkimbi, ukuze kwenziwe ukwakheka okungenalutho ngokuyisisekelo kuvumelane nokwakheka kokwenza, ukuze insimbi ikwazi ukusatshalaliswa ngokufanelekile futhi igcwalise umgodi kahle, kuyadingeka ukuthi kufakwe kuqala okungenalutho emgodini ongenalutho.
- Ukudweba isikhunta eside. Isetshenziselwa ukunciphisa indawo enqamulelayo yengxenye ethile engenalutho ukukhulisa ubude bengxenye. Umdwebo wokudweba uhlukaniswe izinhlobo ezimbili: uhlobo oluvulekile nohlobo oluvaliwe.
- Umngcele we-rolling die. Isetshenziselwa ukunciphisa indawo enqamulelayo yengxenye eyodwa yokungenalutho ukukhulisa indawo enqamulelayo yenye ingxenye, ukuze insimbi isatshalaliswe ngokwendlela yokwakhiwa kwayo. Umgodi oguqulwayo uhlukaniswe izinhlobo ezimbili: uhlobo oluvulekile nohlobo oluvaliwe.
- Ukugoba umgodi wesikhunta. Okokugoba kwenduku okugoqiwe, umgodi wokugoba odingekayo uyadingeka ukugoba okungenalutho.
- Sika umgodi. Kwakha iphehla yommese emakhoneni esikhunta esingenhla nesikhunta esingezansi ukusika insimbi.
Izinzuzo zokwenza okokufa: ukusebenza kahle kokukhiqiza okuphezulu. Lapho kufa ukwakhiwa, ukusonteka kwensimbi kwenziwa emgodini wokufa, ngakho-ke ukwakheka okudingekayo kungatholakala ngokushesha; ingakha ukukholelwa okuyinkimbinkimbi, futhi ingenza ukusatshalaliswa kwensimbi kube okunengqondo ngokwengeziwe, futhi kuthuthukise impilo yesevisi yezingxenye; usayizi we-die forgings Unembe kakhudlwana, ikhwalithi engaphezulu engcono, isabelo esincane semishini; londoloza izinto zensimbi futhi unciphise umthwalo wokusika ukucubungula. Ngaphansi kwesimo senani elanele, izindleko zezingxenye zingancishiswa.
Okubi kanye nemikhawulo yokufa okwenziwe: isisindo sokufa kwe-dieings kukhawulwe ngumthamo wemishini yokufa ejwayelekile, ikakhulukazi ngaphansi kwe-7OKg; umjikelezo wokukhiqiza wokwakha ufile mude futhi izindleko ziphakeme; izindleko zokutshala imali zemishini yokwakha i-die inkulu kunaleyo yokwakhiwa kwamahhala.
Sicela ugcine umthombo nekheli lale ndatshana ukuze uphinde uprintwe: Izinzuzo Nobubi Of Free UKWAKHA Futhi Die UKWAKHA Izindlela
UMinghe Inkampani yeDie Casting anikezelwe ekukhiqizeni nasekuhlinzekeni ikhwalithi nokusebenza okuphezulu Izingxenye Zokulingisa (izingxenye zensimbi zensimbi zokufa zisebenza ikakhulukazi zibandakanya I-Thin-Wall Die Casting,I-Hot Chamber Die Casting,Cold Chamber die Casting), Insizakalo Eyindilinga (Insiza Yokulingisa,ICnc Machining,Ukwenza Okubandayo, Surface Treatment) .Noma ikuphi ukusakazwa kwe-Aluminium die, i-magnesium noma i-Zamak / zinc die casting nezinye izidingo zokuphosa zamukelekile ukuxhumana nathi.
Ngaphansi kokulawulwa kwe-ISO9001 ne-TS 16949, Zonke izinqubo zenziwa ngamakhulu emishini esezingeni eliphakeme yokufa, imishini ye-5-axis, nezinye izikhungo, ezisukela kuma-blasters kuya kumishini yokuwasha ye-Ultra Sonic.Minghe akagcinanga ngemishini esezingeni eliphezulu kepha futhi unobuchwepheshe iqembu lonjiniyela abanolwazi, ama-opharetha nabahloli ukwenza ukwakheka kwekhasimende kugcwaliseke.
Umenzi wenkontileka yokufa kwabasikiwe. Amandla afaka izingxenye ezibandayo ze-aluminium die casting ezivela ku-0.15 lbs. kuye ku-6 lbs., Ukusetha ushintsho olusheshayo, nemishini. Izinsizakalo ezingezwe ngenani zifaka phakathi ukupholisha, ukudlidliza, ukuphazamisa, ukuqhumisa ngokudubula, ukupenda, ukuhlobisa, ukumboza, ukuhlangana nokusetshenziswa kwamathuluzi. Izinto zokusebenza ezisetshenzisiwe zifaka ama-alloys afana no-360, 380, 383, no-413.
I-Zinc die casting design usizo / izinsizakalo zobunjiniyela ezihambisanayo. Umenzi wangokwezifiso we-precision zinc die castings. Ukusakazwa okuncane, ukukhishwa kwengcindezi ephezulu, ukusikeka kwesikhunta esiningi, ukujikijelwa kwesikhunta okuvamile, ukufefa kwamayunithi kanye nokuzimela okuzimele kanye nokuvalwa okuvaliwe komgodi kungenziwa. Ama-Castings angenziwa ngobude nobubanzi obufinyelela ku-24 in. Ku +/- 0.0005 in. Ukubekezelelana.
I-ISO 9001: Umkhiqizi oqinisekisiwe ka-2015 we-die cast magnesium, Amandla afaka i-high-pressure magnesium die casting up to 200 ton chamber hot & 3000 ton cold chamber, designing designing, polishing, molding, machining, powder & liquid paint, QA full with CMM amakhono , inhlangano, ukupakisha nokulethwa.
Kuqinisekiswe i-ITAF16949. Insiza Eyengeziwe Yokulingisa Faka ukukhipha utshalomali,ukuphonsa kwesihlabathi,Ukuphonswa kwamandla, Lost Foam Ekubunjweni,I-Centrifugal Casting,Ukuphoswa Kokuqothula,Permanent Isikhunta Ukulingisa, Amakhono afaka i-EDI, usizo lobunjiniyela, ukumodeliswa okuqinile nokucutshungulwa kwesibili.
Izimboni Zokulingisa Izingxenye Zamacala Ezifundo Zezimoto: Izimoto, Amabhayisikili, Izindiza, Izinsimbi Zomculo, I-Watercraft, Amadivayisi we-Optical, Izinzwa, Amamodeli, Amadivayisi we-elekthronikhi, Ukuvaleka, Amawashi, Imishini, Izinjini, Ifenisha, Ubucwebe, AmaJig, Telecom, Ukukhanyisa, Amadivayisi Wezokwelapha, amadivayisi wezithombe, Amarobhothi, okubaziwe, okokusebenza komsindo, okwezemidlalo, i-Tooling, Amathoyizi nokuningi.
Yini esingakusiza ukuthi uyenze ngokulandelayo?
∇ Iya ekhasini eliyisiqalo For I-Die Casting China
→Izingxenye Zokusakaza-Thola esikwenzile.
→ Izeluleko Ezilinganisiwe Mayelana Izinsizakalo Zokufa Zokusakaza
By Umkhiqizi weMinghe Die Casting | Izigaba: Izindatshana Eziwusizo |Material Omaka: I-Aluminium Casting, Zinc Ukulingisa, Ukulingiswa kweMagnesium, I-Titanium Casting, Insimbi Engagqwali, Brass Ekubunjweni,Ukulingiswa kweBronze,Isakaza ividiyo,Umlando wenkampani,I-Aluminium Die Casting | Amazwana Off