Okuqukethwe Kokulawula Ukungcola KuManganese Iron Alloy
Ukucwengwa kwesithando somlilo kuyingxenye ebalulekile yenqubo yesimanje yokukhiqiza insimbi. Ikhwalithi yensimbi incike kakhulu enqubeni yokucwenga ngaphandle kwesithando.
Ukwengezwa kwe-ferroalloy kuzodlala indima ekunciphiseni nasekuhlanganiseni insimbi encibilikisiwe. Phakathi kwabo, i-manganese ferroalloy yi-ferroalloy enomphumela omkhulu kunayo yonke, inani elikhulu kakhulu futhi eliguquguquka kakhulu.
Izinhlobonhlobo zensimbi zibeka phambili i-phosphorus ephansi, isulfure ephansi, i-titanium ephansi, i-aluminium ephansi, i-nitrogen ephansi, i-oxygen ephansi, i-hydrogen ephansi nezinye izidingo zama-alloys e-manganese iron. Ikhwalithi yama-ferroalloys asuselwa ku-manganese asikwazi ukuhlangabezana nezidingo zezinhlobonhlobo zensimbi. Izinkinga ezisezingeni eliphakeme ezikhona yilezi: okuqukethwe okuphezulu kwe-Ti, Al, P, O, N, no-H kuma-alloys e-ferromanganese; P kuma-alloys we-carbon ferromanganese aphakathi nendawo naphakathi, okuqukethwe kwe-S, O, N, H kuphakeme. Ukulawulwa kokuqukethwe kokungcola okuhlukahlukene kuma-alloys e-manganese iron kufanele kuqiniswe, ikakhulukazi:
1.Gas Okuqukethwe
Njengoba i-nitrogen iphendula ngokushesha ngama-manganese ku-800-1000 ° C, ne-nitrogen nayo iyanda ngesikhathi senqubo yokupholisa, ukukhuphula izinga lokupholisa kunenzuzo ekwehliseni i-nitrogen. Lawula okuqukethwe kwe-H2O (amanzi ahlanganisiwe kanye namanzi e-crystal) wenkokhiso futhi wehlise okuqukethwe okungahambelani kwe-coke, ukunciphisa ukuxhumana phakathi kwe-alloy ne-hydrogen esithandweni somlilo, futhi wehlise okuqukethwe kwe-hydrogen ku-alangan mans iron iron. Ngasikhathi sinye, gwema ukuthintana nomoya omanzi ngenqubo yokugaya, ukuhambisa kanye nokugcina ukuvikela ukusabela kokumunca i-hydrogen kwe-alloy.
2.Ukuqukethwe KweCarbon, Sulphur Ne-Oxygen
Izindlela ezenzekayo zokunciphisa okuqukethwe kwekhabhoni ku-manganese-silicon ferroalloy yilezi: ukuthambisa nokunciphisa ikhabhoni; ukwandisa okuqukethwe kwe-silicon ye-manganese-silicon alloy; okwenziwe nge-slag yokunciphisa i-carbon. Okuqukethwe kwesibabule ku-manganese iron alloy kungancishiswa ngokwenza i-alkaline slag nokuwasha i-slag nokucwenga ingxubevange.
Ngokulungisa kabusha nokucwengisisa, ukufakwa kwe-oxide ku-manganese iron alloy kungantanta ebusweni be-alloy futhi kukhangiswe ngudaka ophezulu. Ngaphezu kwalokho, umgomo nobuchwepheshe bokususa i-deoxidation enqubeni yokwenza insimbi kungasetshenziselwa ukunciphisa ama-alloys e-manganese iron ne-aluminium ne-silicon ukunciphisa okuqukethwe kwe-oxygen.
Okuqukethwe kwe-3.Aluminium ne-Titanium
I-Manganese ferrosilicon alloy iqukethe okuqukethwe okuphezulu kwe-aluminium ne-titanium, futhi indlela yayo yokulawula ukungena esithandweni somlilo nokucwengisisa ngaphandle kwesithando somlilo. Indlela yokuhlanza i-ferrosilicon ingasetshenziselwa ukubhekisela ku-dealuminium ne-detitanium ye-manganese ferrosilicon alloy ngaphandle kwesithando somlilo.
4. Ukulawulwa kokuqukethwe kwePhosphorus
Okuqukethwe kwe-phosphorus yama-manganese-based ferroalloys kulawulwa ngokunciphisa i-phosphorus ezintweni ezingavuthiwe nasekuphoseni ngaphandle kwesithando somlilo. Kunezindlela ezimbili zokunciphisa i-phosphorus ezintweni zokusetshenziswa: i-dephosphorization ye-manganese ore nokuncibilikiswa kwe-phosphorus ephansi kanye ne-slag ecebile ye-manganese. Inqubo yokwenziwa kwe-dephosphorization ye-manganese ore iyinkimbinkimbi, kanti inqubo yokuncibilikisa i-low-phosphorus kanye ne-slag ecebile ye-manganese yinde, futhi izindleko namandla okusetshenziswa kuphezulu. I-Dephosphorization ngaphandle kwesithando somlilo se-ferromanganese ingaba yindlela elula futhi engenzeka kwezomnotho.
Sicela ugcine umthombo nekheli lale ndatshana ukuze uphinde uprintwe: Okuqukethwe Kokulawula Ukungcola KuManganese Iron Alloy
UMinghe Inkampani yeDie Casting anikezelwe ekukhiqizeni nasekuhlinzekeni ikhwalithi nokusebenza okuphezulu Izingxenye Zokulingisa (izingxenye zensimbi zensimbi zokufa zisebenza ikakhulukazi zibandakanya I-Thin-Wall Die Casting,I-Hot Chamber Die Casting,Cold Chamber die Casting), Insizakalo Eyindilinga (Insiza Yokulingisa,ICnc Machining,Ukwenza Okubandayo, Surface Treatment) .Noma ikuphi ukusakazwa kwe-Aluminium die, i-magnesium noma i-Zamak / zinc die casting nezinye izidingo zokuphosa zamukelekile ukuxhumana nathi.
Ngaphansi kokulawulwa kwe-ISO9001 ne-TS 16949, Zonke izinqubo zenziwa ngamakhulu emishini esezingeni eliphakeme yokufa, imishini ye-5-axis, nezinye izikhungo, ezisukela kuma-blasters kuya kumishini yokuwasha ye-Ultra Sonic.Minghe akagcinanga ngemishini esezingeni eliphezulu kepha futhi unobuchwepheshe iqembu lonjiniyela abanolwazi, ama-opharetha nabahloli ukwenza ukwakheka kwekhasimende kugcwaliseke.
Umenzi wenkontileka yokufa kwabasikiwe. Amandla afaka izingxenye ezibandayo ze-aluminium die casting ezivela ku-0.15 lbs. kuye ku-6 lbs., Ukusetha ushintsho olusheshayo, nemishini. Izinsizakalo ezingezwe ngenani zifaka phakathi ukupholisha, ukudlidliza, ukuphazamisa, ukuqhumisa ngokudubula, ukupenda, ukuhlobisa, ukumboza, ukuhlangana nokusetshenziswa kwamathuluzi. Izinto zokusebenza ezisetshenzisiwe zifaka ama-alloys afana no-360, 380, 383, no-413.
I-Zinc die casting design usizo / izinsizakalo zobunjiniyela ezihambisanayo. Umenzi wangokwezifiso we-precision zinc die castings. Ukusakazwa okuncane, ukukhishwa kwengcindezi ephezulu, ukusikeka kwesikhunta esiningi, ukujikijelwa kwesikhunta okuvamile, ukufefa kwamayunithi kanye nokuzimela okuzimele kanye nokuvalwa okuvaliwe komgodi kungenziwa. Ama-Castings angenziwa ngobude nobubanzi obufinyelela ku-24 in. Ku +/- 0.0005 in. Ukubekezelelana.
I-ISO 9001: Umkhiqizi oqinisekisiwe ka-2015 we-die cast magnesium, Amandla afaka i-high-pressure magnesium die casting up to 200 ton chamber hot & 3000 ton cold chamber, designing designing, polishing, molding, machining, powder & liquid paint, QA full with CMM amakhono , inhlangano, ukupakisha nokulethwa.
Kuqinisekiswe i-ITAF16949. Insiza Eyengeziwe Yokulingisa Faka ukukhipha utshalomali,ukuphonsa kwesihlabathi,Ukuphonswa kwamandla, Lost Foam Ekubunjweni,I-Centrifugal Casting,Ukuphoswa Kokuqothula,Permanent Isikhunta Ukulingisa, Amakhono afaka i-EDI, usizo lobunjiniyela, ukumodeliswa okuqinile nokucutshungulwa kwesibili.
Izimboni Zokulingisa Izingxenye Zamacala Ezifundo Zezimoto: Izimoto, Amabhayisikili, Izindiza, Izinsimbi Zomculo, I-Watercraft, Amadivayisi we-Optical, Izinzwa, Amamodeli, Amadivayisi we-elekthronikhi, Ukuvaleka, Amawashi, Imishini, Izinjini, Ifenisha, Ubucwebe, AmaJig, Telecom, Ukukhanyisa, Amadivayisi Wezokwelapha, amadivayisi wezithombe, Amarobhothi, okubaziwe, okokusebenza komsindo, okwezemidlalo, i-Tooling, Amathoyizi nokuningi.
Yini esingakusiza ukuthi uyenze ngokulandelayo?
∇ Iya ekhasini eliyisiqalo For I-Die Casting China
→Izingxenye Zokusakaza-Thola esikwenzile.
→ Izeluleko Ezilinganisiwe Mayelana Izinsizakalo Zokufa Zokusakaza
By Umkhiqizi weMinghe Die Casting | Izigaba: Izindatshana Eziwusizo |Material Omaka: I-Aluminium Casting, Zinc Ukulingisa, Ukulingiswa kweMagnesium, I-Titanium Casting, Insimbi Engagqwali, Brass Ekubunjweni,Ukulingiswa kweBronze,Isakaza ividiyo,Umlando wenkampani,I-Aluminium Die Casting | Amazwana Off