Inqubo yokuqeda ukuvutha kwe-inthanethi ngqo (i-DQ-T) isetshenziswa kancane kancane ukukhiqiza insimbi enamandla amakhulu, eqeda inqubo yokuvuselela ikhambi yokwelashwa kwendabuko, futhi inikeze ukudlala okugcwele endimeni yokuhlanganisa izinto ukwenza ngcono ukuqina, okuthuthuka kakhulu ukusebenza kahle kokukhiqiza kanye nomnotho wamapuleti ensimbi. .
I-HSLA-80 (560 MPa) equkethe ithusi, ama-steels ochungechunge we-HSLA-100 (690MPa) anokusebenza okuhle kwe-welding. Ngesikhathi senqubo yokushisa, ukuqiniswa kwezulu kwezinhlayiya ze-ε-Cu kwenza lolu chungechunge lwezinsimbi lube namandla amakhulu, futhi ingxenyenamba yesisindo sekhabhoni ephansi ibenza babe bahle kakhulu kubulukhuni bokushisa okuphansi nokusebenza kwe-welding.
Izazi ezivela kuJiangsu Iron and Steel Research Institute zifunde insimbi yomkhumbi enamandla okuvuna amakhulu kune-785MPa, yahlola ijika layo eliguqukayo lokupholisa eliqhubekayo (CCT), futhi yafunda ukugoqwa okulawulwayo + kokucima okuqondile + kwe-tempering (DQ- T) ngemuva kokwelashwa kwenqubo. Imiphumela ikhombisa ukuthi ukwakheka kwepuleti lensimbi elicishiwe ngqo (i-DQ) yi-lath martensite (LM), futhi izakhi zethusi ne-niobium zihlakazekile futhi zashiswa ngemuva kokufutheka.
Amandla wensimbi yensimbi emnene ku-500 ℃ yiyona ephezulu kakhulu, futhi ukuqina komthelela (KV2) yikhona okuphansi kakhulu. Ipuleti lensimbi lifudumele ku-710 ℃, ukwakheka kwalo yi-martensite yesibili (SLM) + ferrite, amandla esivuno (Re) yi-810MPa, amandla we-tensile (Rm) yi-1066MPa, ne-elongation (A) ingu-17%. I-KV2 ingu-97J ngo- -80 ℃, ethola ukufana okuhle kakhulu kwamandla nobulukhuni.
Sicela ugcine umthombo nekheli lale ndatshana ukuze uphinde uprintwe:Ukusebenza Kwe-785MPa Low-Carbon Copper-Bearing Ship Plate Steel
UMinghe Inkampani yeDie Casting anikezelwe ekukhiqizeni nasekuhlinzekeni ikhwalithi nokusebenza okuphezulu Izingxenye Zokulingisa (izingxenye zensimbi zensimbi zokufa zisebenza ikakhulukazi zibandakanya I-Thin-Wall Die Casting,I-Hot Chamber Die Casting,Cold Chamber die Casting), Insizakalo Eyindilinga (Insiza Yokulingisa,ICnc Machining,Ukwenza Okubandayo, Surface Treatment) .Noma ikuphi ukusakazwa kwe-Aluminium die, i-magnesium noma i-Zamak / zinc die casting nezinye izidingo zokuphosa zamukelekile ukuxhumana nathi.
Ngaphansi kokulawulwa kwe-ISO9001 ne-TS 16949, Zonke izinqubo zenziwa ngamakhulu emishini esezingeni eliphakeme yokufa, imishini ye-5-axis, nezinye izikhungo, ezisukela kuma-blasters kuya kumishini yokuwasha ye-Ultra Sonic.Minghe akagcinanga ngemishini esezingeni eliphezulu kepha futhi unobuchwepheshe iqembu lonjiniyela abanolwazi, ama-opharetha nabahloli ukwenza ukwakheka kwekhasimende kugcwaliseke.
Umenzi wenkontileka yokufa kwabasikiwe. Amandla afaka izingxenye ezibandayo ze-aluminium die casting ezivela ku-0.15 lbs. kuye ku-6 lbs., Ukusetha ushintsho olusheshayo, nemishini. Izinsizakalo ezingezwe ngenani zifaka phakathi ukupholisha, ukudlidliza, ukuphazamisa, ukuqhumisa ngokudubula, ukupenda, ukuhlobisa, ukumboza, ukuhlangana nokusetshenziswa kwamathuluzi. Izinto zokusebenza ezisetshenzisiwe zifaka ama-alloys afana no-360, 380, 383, no-413.
I-Zinc die casting design usizo / izinsizakalo zobunjiniyela ezihambisanayo. Umenzi wangokwezifiso we-precision zinc die castings. Ukusakazwa okuncane, ukukhishwa kwengcindezi ephezulu, ukusikeka kwesikhunta esiningi, ukujikijelwa kwesikhunta okuvamile, ukufefa kwamayunithi kanye nokuzimela okuzimele kanye nokuvalwa okuvaliwe komgodi kungenziwa. Ama-Castings angenziwa ngobude nobubanzi obufinyelela ku-24 in. Ku +/- 0.0005 in. Ukubekezelelana.
I-ISO 9001: Umkhiqizi oqinisekisiwe ka-2015 we-die cast magnesium, Amandla afaka i-high-pressure magnesium die casting up to 200 ton chamber hot & 3000 ton cold chamber, designing designing, polishing, molding, machining, powder & liquid paint, QA full with CMM amakhono , inhlangano, ukupakisha nokulethwa.
Kuqinisekiswe i-ITAF16949. Insiza Eyengeziwe Yokulingisa Faka ukukhipha utshalomali,ukuphonsa kwesihlabathi,Ukuphonswa kwamandla, Lost Foam Ekubunjweni,I-Centrifugal Casting,Ukuphoswa Kokuqothula,Permanent Isikhunta Ukulingisa, Amakhono afaka i-EDI, usizo lobunjiniyela, ukumodeliswa okuqinile nokucutshungulwa kwesibili.
Izimboni Zokulingisa Izingxenye Zamacala Ezifundo Zezimoto: Izimoto, Amabhayisikili, Izindiza, Izinsimbi Zomculo, I-Watercraft, Amadivayisi we-Optical, Izinzwa, Amamodeli, Amadivayisi we-elekthronikhi, Ukuvaleka, Amawashi, Imishini, Izinjini, Ifenisha, Ubucwebe, AmaJig, Telecom, Ukukhanyisa, Amadivayisi Wezokwelapha, amadivayisi wezithombe, Amarobhothi, okubaziwe, okokusebenza komsindo, okwezemidlalo, i-Tooling, Amathoyizi nokuningi.
Yini esingakusiza ukuthi uyenze ngokulandelayo?
∇ Iya ekhasini eliyisiqalo For I-Die Casting China
→Izingxenye Zokusakaza-Thola esikwenzile.
→ Izeluleko Ezilinganisiwe Mayelana Izinsizakalo Zokufa Zokusakaza
By Umkhiqizi weMinghe Die Casting | Izigaba: Izindatshana Eziwusizo |Material Omaka: I-Aluminium Casting, Zinc Ukulingisa, Ukulingiswa kweMagnesium, I-Titanium Casting, Insimbi Engagqwali, Brass Ekubunjweni,Ukulingiswa kweBronze,Isakaza ividiyo,Umlando wenkampani,I-Aluminium Die Casting | Amazwana Off