Ukusebenza Nokunakekelwa Kwesisetshenziswa Esiqhubekayo seCaster
Ukusakaza okuqhubekayo kuyindlela yokukhiqiza esebenza kahle kakhulu. Umshini wokusakaza oqhubekayo yigama elijwayelekile lemishini eqhubeka ngokuqeda ukwahlukaniswa nokukhishwa kwensimbi encibilikisiwe eyakha (ukuthulula, ukufingqa).
Ngesikhathi senqubo yokukhiqiza, ukusebenza kahle nokuzinzile kwemishini kuthuthukisa kakhulu ukusebenza kahle kokukhiqiza futhi kunciphisa izindleko zokukhiqiza, kepha futhi kuletha ubunzima ekukhiqizeni nasekulondolozeni. Naka okulandelayo ngesikhathi sesondlo:
Ukupholisa uhlelo lwamanzi
Amanzi "yigazi" lomshini wokulingisa oqhubekayo, oqinisekisa ukupholisa okwanele, okunganciphisa ukucindezela okushisayo kwe-roller, kugweme ukugoba kwe-roller, futhi kuthuthukise ukusebenza kozinzo.
- 1) Isondlo: Ngesikhathi senqubo yesondlo, yenza ukuhlolwa kwengcindezi kupayipi lamanzi okupholisa. Ukumelana kwengcindezi kwepayipi ngalinye kuhlangabezana nengcindezi edingekayo ekukhiqizweni okuvamile futhi kugcina isikhathi esibekiwe. Bheka ngokucophelela isimo sepayipi lonke nezingxenye ezixhumayo ukuqinisekisa ukuthi uhlelo lwamanzi okupholisa Ipayipi aliphazamiseki futhi akukho ukuvuza.
- 2) Esizeni: Hlela ukuhlolwa kwamaphayiphi wesistimu yokupholisa ngesikhathi sokuvala nokucisha, futhi ubhekane nesikhathi esifanele ngamapayipi avuzayo noma afihliwe, izimvu zamanzi, njll. Qinisa ukuhlolwa kwekhwalithi yamanzi ukuvimbela ukuvuza okukhulu kwamanzi okungenakulungiswa ngenxa yenkinga ukuvaleka kwamapayipi noma ukugqwala kwamapayipi ngenxa yekhwalithi yamanzi engeyinhle, ukuze kugwenywe izindleko ezingadingekile lapho imishini isetshenziswa online.
Uwoyela omile uhlelo lokuthambisa
I-lubricant "ukudla" komshini wokusakaza oqhubekayo, okuqinisekisa ukusebenza kahle komshini wokusakaza oqhubekayo.
- 1) Isondlo: Ngaphambi kwesondlo, qinisekisa ikhwalithi yomhlangano we-caster roll eqhubekayo, gcwalisa umqulu wonyawo ngenani elifanele lamafutha omile, bese wenza isivivinyo somfutho owomile. Ipayipi lokuthambisa uwoyela owomile kufanele ligcinwe lingavinjelwe futhi akumele kube nezindawo zokuvuza.
- 2) Esizeni: Kuyadingeka ukuqinisekisa ukuthi ama-roller womshini wokulingisa oqhubekayo asebenza ngokuguquguqukayo, futhi awekho ama-roller afile.
3. Uhlelo lwe-Hydraulic
Gcina uhlelo lwe-hydraulic luvuza futhi lusebenza kahle ukuqinisekisa ukukhiqizwa okuhle komshini wokusakaza oqhubekayo.
- 1) Isondlo: Faka esikhundleni ishubhu ye-hydraulic yekhwalithi engafaneleki ngesikhathi; isilinda esiqinisayo nesilinda esicindezelayo kufanele sicindezelwe ngawodwana futhi sigcinwe isikhathi esishiwo; ukuhlolwa kwengcindezi kufanele kwenziwe futhi ngemuva kokuthi wonke umshini usulungile.
- 2) Esizeni: Qinisa ukuhlolwa kwekhwalithi kawoyela kawoyela wokubacindezela ukuqinisekisa ukuhlanzeka kukawoyela wokubacindezela nokuvimbela izingxenye zokunyakaza ukuthi zingqubuzana futhi zithinte ukukhiqizwa.
I-4. Okunye
- 1) Qinisekisa ikhwalithi yezingxenye zokhiye ezibalulekile nezinto zokusetshenziswa, futhi ungasebenzisi izingxenye ezisele nezinto zokusetshenziswa ezinekhwalithi engafanelekile noma umjikelezo wokuphila omfushane.
- 2) Qinisekisa ikhwalithi yokugcinwa kwemishini. Bheka izingxenye ezisele zemishini engaxhunyiwe ku-inthanethi. Ezingxenyeni ezisebenzisekayo, yenza ukugcinwa okujwayelekile njengokuwehla nokugcoba amafutha; izingxenye ezilungisekayo kufanele zilungiswe ngokuya ngezinga lokulimala nezidingo zomsebenzi; ngezingxenye ezilahliwe ezingalungiseki, Scrap ngokushesha bese ushintsha ngezingxenye ezintsha.
Sicela ugcine umthombo nekheli lale ndatshana ukuze uphinde uprintwe: Ukusebenza Nokunakekelwa Kwesisetshenziswa Esiqhubekayo seCaster
UMinghe Inkampani yeDie Casting anikezelwe ekukhiqizeni nasekuhlinzekeni ikhwalithi nokusebenza okuphezulu Izingxenye Zokulingisa (izingxenye zensimbi zensimbi zokufa zisebenza ikakhulukazi zibandakanya I-Thin-Wall Die Casting,I-Hot Chamber Die Casting,Cold Chamber die Casting), Insizakalo Eyindilinga (Insiza Yokulingisa,ICnc Machining,Ukwenza Okubandayo, Surface Treatment) .Noma ikuphi ukusakazwa kwe-Aluminium die, i-magnesium noma i-Zamak / zinc die casting nezinye izidingo zokuphosa zamukelekile ukuxhumana nathi.
Ngaphansi kokulawulwa kwe-ISO9001 ne-TS 16949, Zonke izinqubo zenziwa ngamakhulu emishini esezingeni eliphakeme yokufa, imishini ye-5-axis, nezinye izikhungo, ezisukela kuma-blasters kuya kumishini yokuwasha ye-Ultra Sonic.Minghe akagcinanga ngemishini esezingeni eliphezulu kepha futhi unobuchwepheshe iqembu lonjiniyela abanolwazi, ama-opharetha nabahloli ukwenza ukwakheka kwekhasimende kugcwaliseke.
Umenzi wenkontileka yokufa kwabasikiwe. Amandla afaka izingxenye ezibandayo ze-aluminium die casting ezivela ku-0.15 lbs. kuye ku-6 lbs., Ukusetha ushintsho olusheshayo, nemishini. Izinsizakalo ezingezwe ngenani zifaka phakathi ukupholisha, ukudlidliza, ukuphazamisa, ukuqhumisa ngokudubula, ukupenda, ukuhlobisa, ukumboza, ukuhlangana nokusetshenziswa kwamathuluzi. Izinto zokusebenza ezisetshenzisiwe zifaka ama-alloys afana no-360, 380, 383, no-413.
I-Zinc die casting design usizo / izinsizakalo zobunjiniyela ezihambisanayo. Umenzi wangokwezifiso we-precision zinc die castings. Ukusakazwa okuncane, ukukhishwa kwengcindezi ephezulu, ukusikeka kwesikhunta esiningi, ukujikijelwa kwesikhunta okuvamile, ukufefa kwamayunithi kanye nokuzimela okuzimele kanye nokuvalwa okuvaliwe komgodi kungenziwa. Ama-Castings angenziwa ngobude nobubanzi obufinyelela ku-24 in. Ku +/- 0.0005 in. Ukubekezelelana.
I-ISO 9001: Umkhiqizi oqinisekisiwe ka-2015 we-die cast magnesium, Amandla afaka i-high-pressure magnesium die casting up to 200 ton chamber hot & 3000 ton cold chamber, designing designing, polishing, molding, machining, powder & liquid paint, QA full with CMM amakhono , inhlangano, ukupakisha nokulethwa.
Kuqinisekiswe i-ITAF16949. Insiza Eyengeziwe Yokulingisa Faka ukukhipha utshalomali,ukuphonsa kwesihlabathi,Ukuphonswa kwamandla, Lost Foam Ekubunjweni,I-Centrifugal Casting,Ukuphoswa Kokuqothula,Permanent Isikhunta Ukulingisa, Amakhono afaka i-EDI, usizo lobunjiniyela, ukumodeliswa okuqinile nokucutshungulwa kwesibili.
Izimboni Zokulingisa Izingxenye Zamacala Ezifundo Zezimoto: Izimoto, Amabhayisikili, Izindiza, Izinsimbi Zomculo, I-Watercraft, Amadivayisi we-Optical, Izinzwa, Amamodeli, Amadivayisi we-elekthronikhi, Ukuvaleka, Amawashi, Imishini, Izinjini, Ifenisha, Ubucwebe, AmaJig, Telecom, Ukukhanyisa, Amadivayisi Wezokwelapha, amadivayisi wezithombe, Amarobhothi, okubaziwe, okokusebenza komsindo, okwezemidlalo, i-Tooling, Amathoyizi nokuningi.
Yini esingakusiza ukuthi uyenze ngokulandelayo?
∇ Iya ekhasini eliyisiqalo For I-Die Casting China
→Izingxenye Zokusakaza-Thola esikwenzile.
→ Izeluleko Ezilinganisiwe Mayelana Izinsizakalo Zokufa Zokusakaza
By Umkhiqizi weMinghe Die Casting | Izigaba: Izindatshana Eziwusizo |Material Omaka: I-Aluminium Casting, Zinc Ukulingisa, Ukulingiswa kweMagnesium, I-Titanium Casting, Insimbi Engagqwali, Brass Ekubunjweni,Ukulingiswa kweBronze,Isakaza ividiyo,Umlando wenkampani,I-Aluminium Die Casting | Amazwana Off