Izinga eliphelele ukwamukelwa isikhunta emlandweni!
1. Ukubukeka, ubukhulu nosayizi womkhiqizo obunjiwe
1. Amaphutha ebusweni bomkhiqizo awavunyelwe: ukungabi bikho kwempahla, okushisiwe, okumhlophe okuphezulu, umugqa omhlophe, ukuphakama, ukushaya ibhalansi, ukwenza mhlophe (noma ukuqhekeka, ukuphuka), ukubhaka, nemibimbi. .
2. Ukushisela uphawu: Ngokuvamile, ubude bensimbi eyindilinga yomgodi we-perforation awudluli u-5mm, futhi ubude bamaphetshana we-perforation weld emise okhethekile abangaphansi kuka-15mm, futhi amandla we-weld mark angadlula ukuhlolwa kokuphepha okusebenzayo. .
3. Shrinkage: I-Shrinkage ayivunyelwe ezindaweni ezisobala zokubonakala, futhi ukuncipha okuncane kuvunyelwe ezindaweni ezingabonakali (hhayi ukuzwa imizwa). .
4. Ngokuvamile, isicaba semikhiqizo emincane ingaphansi kuka-0.3mm. Uma kunezidingo zomhlangano, izidingo zomhlangano kufanele ziqinisekiswe.
5. Akufanele kube khona izintambo zomoya noma izimbali ezibonakalayo ngokubonakala okusobala, futhi umkhiqizo kufanele ngokuvamile ungabi nawo amagwebu omoya.
6. Isimo sejiyomethri nokunemba kobukhulu bomkhiqizo kufanele kuhlangabezane nezidingo zomdwebo wesikhunta osemthethweni futhi osebenzayo (noma ifayela le-3D). Ukubekezelelana komkhiqizo kufanele kusekelwe kumgomo wokubekezelelana. Ukubekezelelana kosayizi we-shaft ukubekezelelana okungalungile, futhi ukubekezelelana kosayizi wembobo ukubekezelelana okuhle. Ikhasimende linakho njengoba kudingeka, njengoba kudingeka.
7. Ubukhulu bodonga lomkhiqizo: Ubukhulu bomdonga womkhiqizo ngokuvamile budingeka ukuba bube nobukhulu besilinganiso sodonga, ukujiya kodonga okungekho isilinganiso kufanele kuhlangabezane nezidingo zomdwebo, futhi ukubekezelelana kufanele kube -0.1mm ngokuya ngezimpawu zesikhunta.
8. Ukuhlanganiswa komkhiqizo: ukuhlangana kwegobolondo kanye nokuhlanganiswa kwegobolondo phansi: ukungahambi kahle komhlaba kungaphansi kuka-0.1mm, futhi akufanele kube khona ukuklwebheka. Izimbobo, imiphini kanye nendawo equkethe izidingo ezihambisanayo kufanele iqinisekise isikhathi sokuhambisana nokusetshenziswa.
Okwesibili, ukuvela kwesikhunta
1. Okuqukethwe kupuleti legama lesikhunta kuqediwe, izinhlamvu zicacile, futhi ukuhleleka kucocekile.
2. I-nameplate kufanele ilungiswe onyaweni lwesikhunta eduze kwesifanekiso kanye ne-angle angle. I-nameplate inokwethenjelwa futhi akulula ukuyikhipha.
3. Umbhobho wamanzi opholile kufanele wenziwe ngombhobho wamanzi webhulashi, uma ikhasimende lidinga okuhlukile, sicela ulandele izidingo. 4. Umbhobho wamanzi opholile akufanele uphume ebusweni besisekelo sesikhunta
5. Umbhobho wamanzi opholile udinga ukuthi ucutshungulwe ngomunye umkhiqizo. Ububanzi be-counterbore ngu-25mm, 30mm no-35mm. I-orifice ihlanjululwe futhi i-chamfer kufanele ifane. .
6. Umbhobho wamanzi opholile kufanele umakwe ukungena nokuphuma.
7. Maka izinhlamvu zesiNgisi nezinombolo kufanele zibe ngaphezu kuka-5/6, futhi indawo kufanele ibe ngu-10mm ngqo ngaphansi kompompi. Umbhalo wesandla kufanele ucace, ube muhle, ucoceke futhi uhlukaniswe ngokulinganayo.
8. Izesekeli zesikhunta akufanele zithinte ukuphakamisa nokugcina isikhunta. Ngesikhathi sokufakwa, kunama-cylinders ka-oli adaluliwe, ompompi, indlela yokusetha kabusha kabusha, njll, okufanele ivikelwe yimilenze esekelayo.
9. Ukufakwa komlenze wokusekelwa kufanele kulungiswe kusisekelo sesikhunta ngezikulufo ezidlula emlenzeni wokusekela, futhi umlenze wokusekela omude ngokweqile ungaboshelwa kusisekelo sesikhunta ngekholamu yangaphandle eyenziwe ngomshini.
10. Usayizi womgodi we-ejector wesikhunta kufanele uhlangabezane nezidingo zomshini obunjiwe womjovo womjovo. Ngaphandle kwesikhunta esincane, isikhungo esisodwa asinakusetshenziselwa ukukhipha.
11. Iringi yokuma kufanele ilungiswe futhi ithembeke. Ububanzi bendandatho ngu-100mm no-250mm. Iringi yokuma iphakeme nge-10-20mm kunepuleti eliphansi. Ngaphandle kokuthi kucelwe ngenye indlela ngamakhasimende.
12. Ubukhulu bangaphandle besikhunta kufanele buhlangabezane nezidingo zomshini obunjiwe womjovo.
13. Kwisikhunta esinezidingo zokuqondisa, umcibisholo kufanele usetshenziselwe ukukhombisa inkomba yokufaka kuthempulethi engaphambili noma ithempulethi engemuva. Kufanele kube ne- "UP" eceleni komcibisholo. Umcibisholo nombhalo womabili kuphuzi kanti ukuphakama kwefonti kungu-50 mm.
14. Ubuso besisekelo sesikhunta akufanele sibe nemigodi, izimpawu zokugqwala, izindandatho ezingasasebenzi, umusi wamanzi ngaphakathi nangaphandle, izimbobo zikawoyela, njll, kanye nokukhubazeka okuthinta ukubukeka.
15. Isikhunta kufanele kube lula ukuphakamisa nokuhambisa, futhi izingxenye zesikhunta akumele zihlukaniswe ngesikhathi sokuphakanyiswa, futhi indandatho yokuphakamisa akumele iphazamise umbhobho wamanzi, isilinda samafutha, induku yokusetha kabusha, njll.
3. Isikhunta impahla kanye nobulukhuni
1. Isisekelo sesikhunta kufanele sibe isisekelo sesikhunta esijwayelekile esivumelana nezinga.
2. Izingxenye ezakha isikhunta nohlelo lwegeyithi (okufakiwe okuyisisekelo, okuhambayo nokuhleliwe, ukufakwa okugudlukayo, izigaxa ezihlukanisiwe, izinduku zokuphusha, imikhono ye-sprue) zenziwe ngezinto zokusebenza ezinokusebenza okuphezulu kune-40Cr.
3. Lapho kubunjwa oplastikhi abonakalisa isikhunta, izingxenye ezibunjiwe kufanele zenziwe ngezinto ezingamelana nokugqwala, noma indawo yokubumba kufanele ithathe izinyathelo zokulwa nokugqwala.
4. Ubulukhuni bezingxenye ezibunjiwe akufanele bube ngaphansi kuka-50HRC, noma ubulukhuni bokwelashwa kokuqina kwendawo kufanele kube ngaphezulu kuka-600HV.
Okune, khipha, setha kabusha, khipha i-ferrule, khipha
1. Ukukhishwa kufanele kube bushelelezi, ngaphandle kokuminyana, futhi ngaphandle komsindo ongajwayelekile.
2. Indawo engaphezulu ethambekele kufanele ipholishwe, futhi indawo engaphezulu ethambekele ingaphansi kwengaphezulu.
3. Izingxenye ezislayidayo kufanele zinikezwe i-groove kawoyela, futhi ingaphezulu lidinga ukufakwa i-nitrided, nobulukhuni bendawo ngemuva kokwelashwa yi-HV700 noma ngaphezulu.
4. Zonke izinduku ze-ejector kufanele zibe nokuma kwe-stop-rotation, futhi induku ngayinye ye-ejector kufanele ibe nezinombolo.
5. Ibanga lokukhishwa kufanele lilinganiselwe nge-block block
6. Izingxenye ezijwayelekile kufanele zisetshenziselwe intwasahlobo ebuyayo, futhi zombili iziphetho zentwasahlobo akufanele zipholishwe noma zinqunywe.
7. Isilayida nokudonsa okuyisisekelo kufanele kube nomkhawulo wokushaywa unhlangothi, isilayidi esincane sinqunyelwe entwasahlobo, uma intwasahlobo ingalungile ukufaka, isikulufa sikathayela singasetshenziswa; ukudonsa okuyisilinda okuyisisekelo kufanele kube neswishi yokushaywa unhlangothi.
8. Ngokuvamile, okuthunyelwe okuqondiswayo okusetshenzisiwe kusetshenziselwa ukudonsa okuyisisekelo kwesilayida, futhi i-engeli yomhlahlandlela othambekele kufanele ibe ngu-2 ° ~ 3 ° incane kune-engeli yendawo yokukhiya isilayida. Uma ukushaywa yisilayida kukude kakhulu, isilinda samafutha kufanele sisetshenziselwe ukudweba.
9. Lapho indawo yokuphela kwengxenye eyindilinga yokudonsa eyinhloko imboziwe, isilinda kufanele ifakwe indlela yokuzikhiya.
10. Kufanele kube khona amapuleti amelana nokugqoka ngaphansi kwamaslayidi amakhulu anobubanzi obungaphezu kuka-150 mm. Impahla yepuleti emelana nokugqoka kufanele ibe yi-T8A. Ubulukhuni ngemuva kokwelashwa kokushisa yi-HRC50-55. Ipuleti elingagqoki ingu-0.05-0.1 mm ukuphakama kunendawo enkulu. Vula ithangi likawoyela.
11. Induku ye-ejector akumele iye phezulu naphezulu.
12. Faka ama-barbs endukwini ephezulu, futhi ukuqondiswa kwama-barbs kufanele kungaguquguquki, ukuze ama-barbs kube lula ukuwasusa kumkhiqizo.
13. Ukususwa phakathi komgodi we-ejector pin kanye ne-ejector pin, ubude besigaba sokubeka uphawu, kanye nobukhulu bendawo yomgodi we-ejector pin kufanele kuhambisane nezidingo zamazinga afanele ebhizinisi.
14. Umkhiqizo kufanele ube lula ukuthi opharetha awususe.
15. Lapho umkhiqizo ukhishwa, kulula ukulandela okungaphezulu okuthambekele, futhi induku ephezulu kufanele ivulwe noma igcotshwe.
16. Ibhulokhi ephezulu eboshwe kwinduku ephezulu kufanele iqine futhi ithembeke, ingxenye engeyona eyakhekile ezungeze umjikelezo kufanele icutshungulwe ngomthambeka ka-3 ° ~ 5 °, bese kuthi umngcele ongezansi kufanele ugejwe.
17. Akufanele kube nokufakwa kwensimbi emgodini wokungena kukawoyela esisekelweni sesikhunta.
18. Ubuso bokugcina benduku yokubuya buyisicaba futhi akukho okushisayo kwendawo. Akukho gasket ezansi kwekhanda lombungu, i-welding spot.
19. Ipuleti lesango lezingqimba ezintathu zesikhunta lihamba ngokushelela, futhi ipuleti lesango kulula ukuvula.
20. Izinduku ezintathu zomkhawulo wesikhunta kufanele zihlelwe ezinhlangothini zombili zesikhombisi sokufakwa kwesikhunta, noma amapuleti okudonsa kufanele engezwe kusisekelo sesikhunta ukuvimbela izinduku zomkhawulo zingaphazamisi opharetha.
21. Isifunda sikawoyela nendawo yomoya kufanele ibe bushelelezi, futhi ukusethwa kabusha kwe-hydraulic ejector kufanele kube endaweni.
22. Imbobo yokukhipha kufanele ivulwe ezansi komkhono womhlahlandlela.
23. Akufanele kube khona imvume yokufakwa kwephini lokubeka.
5. Uhlelo lokupholisa nokushisa
1, Uhlelo lokupholisa noma lokushisa kufanele luvulwe ngokuphelele.
2. Uphawu kufanele luthembeke, uhlelo akufanele luvuze ngaphansi kwengcindezi ye-0.5MPa, futhi kulula ukubheka nokulungisa.
3. Usayizi nokuma kwendawo yokubeka uphawu evulwe esisekelweni sesikhunta kufanele kuhlangabezane nezimfuneko zamazinga afanele.
4. Amafutha kufanele asetshenziswe eringini lokufaka uphawu lapho libekwa, futhi kufanele libe ngaphezulu kunobuso besisekelo sesikhunta ngemuva kokufakwa kwaso.
5. Izihlukanisi zesiteshi sokugeleza kwamanzi nakawoyela kufanele zenziwe ngezinto ezingonakalisi kalula.
6. Isikhunta sangaphambili nangemuva kufanele sisebenzise ukuphakelwa kwamanzi okuphakathi.
Isithupha, uhlelo lokuthela
1, Ukuhlelwa kwesango akufanele kuthinte ukubonakala komkhiqizo futhi kuhlangane nomhlangano womkhiqizo.
2. Isigaba somgijimi nobude kufanele baklanywe ngokufanele, futhi inqubo kufanele ifinyezwe ngangokunokwenzeka ngaphansi kwesisekelo sokuqinisekisa ikhwalithi yokwakha, futhi indawo enqamulelayo kufanele incishiswe ukunciphisa isikhathi sokugcwalisa nokupholisa. Ngasikhathi sinye, ukulahleka kwepulasitiki kohlelo lokuthela kufanele kube kuncane.
3. Ingxenye yomgijimi wesikhunta samapuleti amathathu ngemuva kwesikhunta sangaphambili kufanele ibe yi-trapezoidal noma i-semicircular.
4. Isikhunta samapuleti amathathu sinesipeleki ephathekayo epuletini lesango, ububanzi bokungena kwesango kufanele bube ngaphansi kuka-3 mm, futhi ikhanda lebhola linezinyathelo ezi-3 mm ezijulile ezihlehliselwe kupuleti lesango.
5. Induku yokudonsa ibhola kufanele ilungiswe ngokuthembekile, icindezelwe ngaphansi kwendandatho yokuma, ingalungiswa ngezikulufo ezingenakhanda, noma ingacindezelwa ngepuleti lokucindezela.
6. Amasango nabagijimi kufanele kwenziwe ngomshini ngokwezidingo zosayizi wemidwebo, futhi imishini yokugaya nokupholisha ngesandla ayivunyelwe.
7. Isango lephuzu lesango kufanele lihambisane nezidingo zemininingwane.
8. Kufanele kube nesandiso ekugcineni komgijimi njengomgodi obandayo we-slug.
9. I-bople ebunjiwe emise okwe-Z yenduku yokudonsa kufanele ibe nenguquko ebushelelezi.
10. Umgijimi endaweni yokuvalelisa kufanele abe yindilinga, futhi isikhunta sangaphambili nangemuva asikwazi ukwenziwa kabi.
11. Isango elifihlekile endukwini ye-ejector akufanele libe nokuncipha komhlaba.
12. Ububanzi nokujula komgodi we-slug obandayo wemikhiqizo esobala kufanele kuhlangabezane namazinga wedizayini.
13. Isibambo kulula ukusikhipha, alukho uphawu lwesango ekubukekeni komkhiqizo, futhi asikho isibambo esisele enhlanganweni yomkhiqizo.
14. Ngokwesango eligobile le-latent latent, izingxenye ezimbili ze-insert kufanele zibe ne-nitrided, nobulukhuni bendawo bungafinyelela ku-HV700.
Isikhombisa, uhlelo lomgijimi oshisayo
1. Ukuhleleka kwezintambo zomgijimi oshisayo kufanele kube okufanele ukugcinwa kalula, futhi inombolo yezintambo kufanele ibe yincwadi yokuxhumana yomuntu ngamunye.
2. Umgijimi oshisayo kufanele ahlolwe ukuphepha, futhi ukumelana nokuqina komhlaba kufanele kube mkhulu kune-2MW.
3. Izingxenye ezijwayelekile kufanele zamukelwe ikhabethe lokulawula ukushisa, umlomo oshisayo nomgijimi oshisayo.
4. Umkhono omkhulu wokugeleza kwembobo uxhunywe nomgijimi oshisayo onentambo, kanti indawo engezansi ixhumana nomgijimi oshisayo wokufaka uphawu.
5. Umgijimi oshisayo uxhumana kahle nepuleti yokushisa noma induku yokushisa, kanti ipuleti lokushisa lilungiswe ngezikulufo noma izikopelo, futhi indawo ihlangana kahle.
6. I-thermocouple yohlobo lwe-J kufanele isetshenziswe futhi ifaniswe nemitha yokulawula izinga lokushisa.
7. Iqembu ngalinye lezakhi zokushisa kufanele lilawulwe ngama-thermocouples, futhi isikhundla sama-thermocouples kufanele sihlelwe ngokufanele.
8. Umbhobho kufanele uhlangabezane nezidingo zomklamo.
9. Umgijimi oshisayo kufanele abekwe ngokuthembekile, okungenani izikhonkwane ezimbili zokubeka, noma alungiswe ngezikulufo.
10. Kufanele kube nephedi yokuhlukanisa phakathi komgijimi oshisayo nesifanekiso.
11. Iphutha eliphakathi kwamazinga okushisa asethiwe wemitha yokulawula ukushisa kanye nethempelesha yangempela yokubonisa kufanele ibe ngaphansi kuka- ± 5 ° C, futhi ukulawula izinga lokushisa kufanele kube nokuzwela.
12. Umgodi wokufaka umgodi kanye nemibhobho kufanele udlule.
13. Izintambo zomgijimi oshisayo kufanele zihlanganiswe futhi zimbozwe ngepuleti lengcindezi.
14. Kunamasokhethi amabili esincazelo esifanayo, okufanele amakwe ngokucacile.
15. Intambo yokulawula kufanele ishaywe futhi ingalimali.
Ukwakheka kwekhabethe lokulawula ukushisa kunokwethenjelwa, futhi nezikulufo azikhululekile.
17. Isokhethi lifakwe kwi-bakelite futhi alikwazi ukweqa ubukhulu obukhulu besifanekiso.
Izintambo akumele zivezwe ngaphandle kwesikhunta.
19. Zonke izindawo lapho umgijimi oshisayo noma ithempulethi ixhumana khona nezintambo kufanele kube nezinguquko eziyindilinga.
20. Ngaphambi kokuba ithempulethi ihlanganiswe, ayikho isekhethi evulekile noma isifunda esifushane kuzo zonke izifunda.
21. Yonke i-wiring kufanele ixhunywe kahle, ngokusebenza okuhle kokufakwa.
Ngemuva kokuthi isifanekiso sesifakiwe futhi saboshwa, wonke amasekethe kufanele ahlolwe futhi nge-multimeter.
8. Ukwakha ingxenye, indawo yokuhlukanisa, indawo yokukhipha
1. Akufanele kube khona ukungalingani, imigodi, ukugqwala nezinye izinkinga ezithinta ukubonakala ebusweni besikhunta sangaphambili nangemuva.
2. Ukufaka kufaniswe nohlaka lwesikhunta, futhi kufanele kube khona imvume engaphansi kuka-1 mm emakhoneni ayindilinga.
3. Indawo yokuvalelisa igcinwa ihlanzekile futhi ihlelekile. Alikho isondo lokugaya eliphathekayo ukugwema izimbotshana, futhi ingxenye yokufaka uphawu ayinazo izifaca.
4. Ukujula kwe-groove yokukhipha kufanele kube ngaphansi kwenani lokuchichima kwepulasitiki.
5. Ucwaningo kanye nokusatshalaliswa kokufakwa kufanele kube khona, ngokubekwa bushelelezi nokubekwa okuthembekile.
6. Okufakwa, okufakwa, njll. Kufanele kubekwe kahle futhi kulungiswe, izingcezu eziyindilinga kufanele zivinjelwe ukuthi zishintshane, futhi akumele kubekwe amashidi ethusi noma ensimbi ngaphansi kokufakwa.
7. Ubuso bokugcina benduku ye-ejector buhambisana nengqikithi.
8. Ingxenye eyakhayo yesikhunta sangaphambili nangemuva ayinakho ukukhubazeka njengama-undercuts nama-chamfers.
9. Izimbambo kufanele zikhishwe ngaphandle ngokushelela.
10. Ngemikhiqizo yesikhunta esinemigqa eminingi, izingxenye ezingakwesokunxele nezingakwesokudla ziyalingana, futhi kufanele kukhonjiswe uL noma uR. Uma ikhasimende linezidingo zesikhundla nosayizi, kufanele lihlangabezane nezidingo zamakhasimende. Ngokuvamile, engeza lapho kungathinti ukubukeka nomhlangano. Usayizi wefonti ngu-1/8.
11. Ubuso bokubambelela kwesisekelo sesikhunta kufanele busendaweni, futhi kufanele kuthintwe indawo engaphezu kuka-75% wendawo.
12. Izinduku ze-ejector kufanele zihlelwe eduze kwezindonga ezisemaceleni futhi eceleni kwezimbambo nabaphathi, futhi kufanele kusetshenziswe izinduku ezinkulu ze-ejector.
13. Ezingxenyeni ezifanayo, izinombolo 1, 2, 3, njll.
14. Indawo ngayinye yokuxhumana, indawo engenayo, nendawo yokuhlukanisa kufanele icwaningwe futhi ifaniswe endaweni yayo.
15. Ingxenye yokuvala indawo yokuvala kufanele ihlangabezane namazinga wedizayini. I-10-20mm yezikhunta ezisemaphakathi, i-30-50 mm yezikhunta ezinkulu, futhi izingxenye ezisele ziklanyelwe ukugwema izikhala ezingenalutho.
16. Ukuthungwa kwesikhumba kanye ne-sandblasting kufanele kuhlangabezane nezidingo zamakhasimende ngokulinganayo.
17. Ngemikhiqizo enezidingo zokubukeka, izikulufo emikhiqizweni kufanele zibe nezinyathelo zokulwa nokuncipha.
18. Amapayipi kaJack kufanele asetshenziselwe amakholomu wesikulufu ngokujula okungaphezu kwama-20 mm.
19. Ubukhulu bodonga lomkhiqizo kufanele bufane, futhi ukuphambuka kufanele kulawulwe ngaphansi kuka- ± 0.15 mm.
20. Ububanzi bezimbambo kufanele bube ngaphansi kuka-60% wobukhulu bodonga lwangaphandle olungaphandle
21. Izinhlamvu ezifakiwe ophahleni oluthambekele nesilayida kufanele zibe nendlela yokulungisa ethembekile.
22. Isikhunta sangaphambili sifakwa kwisikhunta sangemuva noma isikhunta sangemuva sifakwa kwisikhunta sangaphambili, futhi izinhlangothi kufanele zikhiywe ngamabhanoyi athambekele futhi kwenziwe ngomshini ukugwema umoya.
Isishiyagalolunye, inqubo yokukhiqiza umjovo wokubumba
1, Isikhunta kufanele sibe nokuqina komkhiqizo wokujova umjovo nokuphindaphindwa kwenqubo yokulungiswa kwepharamitha ngaphakathi kobubanzi bezimo ezijwayelekile zenqubo yokujova.
2.Ingcindezi yomjovo ngesikhathi sokukhiqizwa komjovo wesikhunta kufanele ngokuvamile ibe ngaphansi kuka-85% womshini wokujola womshini wokulinganisa owenziwe ngomshini.
3. Ijubane lomjovo womkhiqizo wokujova umjovo wesikhunta, ijubane lomjovo we-quarter-quarter stroke alikho ngaphansi kwe-10% yesivinini somjovo esiphezulu esilinganisiwe noma ngaphezulu kwe-90% yesivinini somjovo esiphezulu esilinganisiwe.
4. Ingcindezi ubambe isikhunta ngesikhathi umjovo udini kufanele ngokuvamile ibe ngaphansi kuka-85% we langempela esiphezulu ingcindezi umjovo.
5. Amandla okubamba isikhunta ngesikhathi sokukhiqizwa komjovo wokujova kufanele abe ngaphansi kuka-90% wamandla alinganisiwe okuqinisa imodeli esebenzayo.
6. Ngesikhathi senqubo yokukhiqiza umjovo wokujova, umkhiqizo nempahla yombhobho kufanele kukhishwe kalula futhi ngokuphepha (isikhathi ngokuvamile asikho ngaphezu kwamasekhondi ama-2 lilinye).
7. Kwisikhunta esinokufakwa, ukufakwa kulula ukufakwa futhi okufakwa kulungiswa ngokuthembekile ngesikhathi sokukhiqiza.
10. Ukupakisha nokuhamba
1 Imbobo yesikhunta kufanele ihlanzwe futhi ifuthwe ngamafutha alwa nokugqwala.
2. Izingxenye ezislayidayo kufanele zifakwe i-lubricated.
3. I-thelet ye-sprue bushing kufanele ivalwe ngamafutha.
4. Isikhunta kufanele sinikezwe isiqeshana sokubamba, futhi imininingwane ihlangabezana nezidingo zomklamo.
Izingxenye zokungcebeleka nezingubo zokugqoka kufanele ziphelele, kube nohlu olunemininingwane negama lomphakeli
6. Kufanele kuthathwe izinyathelo zokubeka uphawu ukuvimbela ukuthi izinto zangaphandle zingene emanzini okubumba, uketshezi, igesi, nezindawo zokungena zikagesi;
7. Futha upende ebusweni bangaphandle besikhunta, njengoba kudingwa yikhasimende.
8. Isikhunta kufanele sifakwe emaphaketheni angenawo umswakama, angangeni manzi, nakuma-bump-proof, njengoba kudingwa amakhasimende.
9. Imidwebo yomkhiqizo wesikhunta, imidwebo yesakhiwo, imidwebo yokupholisa nokushisa, imidwebo yomgijimi oshisayo, izingxenye ezisele kanye nemininingwane yabaphakeli bezinto zesikhunta, imiyalo yokusebenza, imibiko yokuhlolwa kwesikhunta, izitifiketi zokuhlolwa kwefektri, kanye nemibhalo kagesi kufanele iphelele.
Sicela ugcine umthombo nekheli lale ndatshana ukuze uphinde uprintwe: Izinga eliphelele ukwamukelwa isikhunta emlandweni!
UMinghe Inkampani yeDie Casting anikezelwe ekukhiqizeni nasekuhlinzekeni ikhwalithi nokusebenza okuphezulu Izingxenye Zokulingisa (izingxenye zensimbi zensimbi zokufa zisebenza ikakhulukazi zibandakanya I-Thin-Wall Die Casting,I-Hot Chamber Die Casting,Cold Chamber die Casting), Insizakalo Eyindilinga (Insiza Yokulingisa,ICnc Machining,Ukwenza Okubandayo, Surface Treatment) .Noma ikuphi ukusakazwa kwe-Aluminium die, i-magnesium noma i-Zamak / zinc die casting nezinye izidingo zokuphosa zamukelekile ukuxhumana nathi.
Ngaphansi kokulawulwa kwe-ISO9001 ne-TS 16949, Zonke izinqubo zenziwa ngamakhulu emishini esezingeni eliphakeme yokufa, imishini ye-5-axis, nezinye izikhungo, ezisukela kuma-blasters kuya kumishini yokuwasha ye-Ultra Sonic.Minghe akagcinanga ngemishini esezingeni eliphezulu kepha futhi unobuchwepheshe iqembu lonjiniyela abanolwazi, ama-opharetha nabahloli ukwenza ukwakheka kwekhasimende kugcwaliseke.
Umenzi wenkontileka yokufa kwabasikiwe. Amandla afaka izingxenye ezibandayo ze-aluminium die casting ezivela ku-0.15 lbs. kuye ku-6 lbs., Ukusetha ushintsho olusheshayo, nemishini. Izinsizakalo ezingezwe ngenani zifaka phakathi ukupholisha, ukudlidliza, ukuphazamisa, ukuqhumisa ngokudubula, ukupenda, ukuhlobisa, ukumboza, ukuhlangana nokusetshenziswa kwamathuluzi. Izinto zokusebenza ezisetshenzisiwe zifaka ama-alloys afana no-360, 380, 383, no-413.
I-Zinc die casting design usizo / izinsizakalo zobunjiniyela ezihambisanayo. Umenzi wangokwezifiso we-precision zinc die castings. Ukusakazwa okuncane, ukukhishwa kwengcindezi ephezulu, ukusikeka kwesikhunta esiningi, ukujikijelwa kwesikhunta okuvamile, ukufefa kwamayunithi kanye nokuzimela okuzimele kanye nokuvalwa okuvaliwe komgodi kungenziwa. Ama-Castings angenziwa ngobude nobubanzi obufinyelela ku-24 in. Ku +/- 0.0005 in. Ukubekezelelana.
I-ISO 9001: Umkhiqizi oqinisekisiwe ka-2015 we-die cast magnesium, Amandla afaka i-high-pressure magnesium die casting up to 200 ton chamber hot & 3000 ton cold chamber, designing designing, polishing, molding, machining, powder & liquid paint, QA full with CMM amakhono , inhlangano, ukupakisha nokulethwa.
Kuqinisekiswe i-ITAF16949. Insiza Eyengeziwe Yokulingisa Faka ukukhipha utshalomali,ukuphonsa kwesihlabathi,Ukuphonswa kwamandla, Lost Foam Ekubunjweni,I-Centrifugal Casting,Ukuphoswa Kokuqothula,Permanent Isikhunta Ukulingisa, Amakhono afaka i-EDI, usizo lobunjiniyela, ukumodeliswa okuqinile nokucutshungulwa kwesibili.
Izimboni Zokulingisa Izingxenye Zamacala Ezifundo Zezimoto: Izimoto, Amabhayisikili, Izindiza, Izinsimbi Zomculo, I-Watercraft, Amadivayisi we-Optical, Izinzwa, Amamodeli, Amadivayisi we-elekthronikhi, Ukuvaleka, Amawashi, Imishini, Izinjini, Ifenisha, Ubucwebe, AmaJig, Telecom, Ukukhanyisa, Amadivayisi Wezokwelapha, amadivayisi wezithombe, Amarobhothi, okubaziwe, okokusebenza komsindo, okwezemidlalo, i-Tooling, Amathoyizi nokuningi.
Yini esingakusiza ukuthi uyenze ngokulandelayo?
∇ Iya ekhasini eliyisiqalo For I-Die Casting China
→Izingxenye Zokusakaza-Thola esikwenzile.
→ Izeluleko Ezilinganisiwe Mayelana Izinsizakalo Zokufa Zokusakaza
By Umkhiqizi weMinghe Die Casting | Izigaba: Izindatshana Eziwusizo |Material Omaka: I-Aluminium Casting, Zinc Ukulingisa, Ukulingiswa kweMagnesium, I-Titanium Casting, Insimbi Engagqwali, Brass Ekubunjweni,Ukulingiswa kweBronze,Isakaza ividiyo,Umlando wenkampani,I-Aluminium Die Casting | Amazwana Off